Home Contact Us
About Us Products Services Enquiry Frequently Asked Questions
AmCon epoxy Paste
AmCon epoxy Kev Coat
AmCon epoxy Underwater Repair Putty
AmCon epoxy Reinforced Repair Putty
AmCon epoxy Pipe Tape white
AmCon Repair Kit
AmCon epoxy Fast Paste
 
AmCon Hi-Temp 1000°C Putty
 
AmCon Portable Blaster c/w Turbo Nozzle
 
AmCon Lab-Metal
AmCon Hi-Temp Lab-Metal
 » Product Instructions
 » Suggested Uses
 » Heat Cure
 » Proven in Powder Coating
 » Lab-Metal or Hi-Temp Lab-Metal
 » Important Tips
AmCon Lab-Solvent
 
AmCon Rust Converter
AmCon Galvax
 
     
 

Proven in Powder Coating
Repair Dents, Voids and Imperfections prior to Powder Coating

 
 
For powder coating processes at temperatures LESS than 350ºF, Lab-metal may be used (even for multiple oven passes). Lab-metal typically air dries within 6 hours (depending upon application thickness and air temperature).

For powder coating processes in which the metal parts will NEVER be subject to temperatures higher than 425ºF, for durations NO LONGER THAN 20 minutes, for NO MORE THAN one oven pass, Lab-metal may be used.

Hi-Temp Lab-metal MUST be used in powder coating processes running at temperatures above 425ºF.

Hi-Temp Lab-metal MUST be used if a part is to be exposed to temperatures above 350ºF for more than 20 minutes in duration (or multiple high-heat exposures).

Hi-Temp Lab-metal MUST be applied in thin layers and allowed to air dry for A MINIMUM OF 24 HOURS, then heat cured as instructed on the product label. (If Hi-Temp Lab-metal is not completely dry when subject to heat, and if the product is not properly heat hardened, outgassing or bubbling is likely to occur).


 
 